This information is supplied as a general guideline. Quite often, the laminating temperature will vary depending upon the type of material you are laminating, the accuracy of your machine's thermostat, and many other factors.
As a general rule, start with a medium temperature. If the pouch still looks cloudy after running it through your machine, laminate it at a slightly higher temperature, and then repeat this process until the pouch is clear. If the temperature is too hot, the pouch will warp, have ripples or have heat bubbles.
| Pouch Thickness | Recommended Temp (no carrier) |
Recommended Temp (with carrier) |
|---|---|---|
| 3 Mil (75 mic) | 230° F (110° C) | 230° F (110° C) |
| 5 Mil (125 mic) | 248° F (120° C) | 248° F (120° C) |
| 7 Mil (175 mic) | 257° F (125° C) | 284° F (140° C) |
| 10 Mil (250 mic) | 284° F (140° C) | 302° F (150° C) |